Interface and Performance of Iron Tailings-Geopolymer Composites
Author:
Affiliation:

1.State Key Laboratory of Mechanical Behavior and System Safety of Traffic Engineering Structures, Shijiazhuang Tiedao University, Shijiazhuang 050043, China;2.School of Materials Science and Engineering, Shijiazhuang Tiedao University, Shijiazhuang 050043, China;3.Hebei Key Laboratory of Advanced Materials for Transportation Engineering and Environment, Shijiazhuang Tiedao University, Shijiazhuang 050043, China

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献 [20]
  • |
  • 引证文献
  • | |
  • 文章评论
    摘要:

    用铁尾矿砂或天然砂配制水泥/地聚物砂浆,并对不同骨料与基体间界面的化学反应、界面过渡区(ITZ)微观结构及砂浆性能进行对比研究.结果表明:掺加铁尾矿砂后,粉煤灰/矿渣地聚物溶液中的Na+、Si4+、Al3+、Ca2+质量浓度均有不同程度降低,其中矿渣地聚物溶液反应速率较快,对骨料表层溶解也有更强的促进作用;铁尾矿砂附近界面过渡区结构明显优于天然河砂,且铁尾矿砂-地聚物砂浆的界面纳米力学性能显著高于铁尾矿砂-水泥砂浆;用铁尾矿砂制备的砂浆强度及抗渗性也均优于天然河砂,这种差异在水泥砂浆中最小,在矿渣地聚物砂浆中最显著,而粉煤灰地聚物砂浆在后期才逐渐凸显出铁尾矿砂的优势.

    Abstract:

    Iron tailings and natural sand were used to prepare cement/geopolymer mortar. The chemical reaction between the fine aggregate and the matrix, microstructure of interfacial transition zone (ITZ), strength and impermeability of mortars were studied. The results show that the mass concentrations of Na+, Si4+, Al3+ and Ca2+ in both geopolymer solutions decrease after adding iron tailings powder. The reaction rate in the slag-based geopolymer solution is faster, it plays a stronger role in promoting effect on the dissolution of surface layer of aggregate. The structure of ITZ near the iron tailings is obviously better than that of natural sand, especially in geopolymer mortar. The interfacial nanomechanical performance of iron tailing-geoploymer are significantly higher than that of iron tailing-cement mortar. The strength and impermeability of iron tailings mortar are also better than that of natural sand mortar. The difference is the smallest for cement mortar, and the most significant for slag-based geopolymer mortar, while for the fly ash-based geopolymer mortar the advantage of iron tailings can be seen only in the later stage.

    表 1 原材料的化学组成Table 1 Chemical compositions of raw materials
    表 2 水泥和地聚物砂浆的配合比Table 2 Mix proportions of geopolymer mortar
    图1 不同溶液加入铁尾矿砂后的离子质量浓度变化Fig.1 Changes of ion concentration after adding iron tailings into different solutions
    图2 不同砂浆7 d龄期界面过渡区的SEM-EDS图Fig.2 SEM-EDS images of the ITZ in different kinds of mortar at 7 d age
    图3 龄期为7 d时的砂浆界面过渡区纳米压痕测试结果Fig.3 Nano indentation test results of mortar ITZ at 7 d age
    图4 不同龄期砂浆的抗压强度与抗折强度Fig.4 Compressive strength and flexural strength of mortar at different ages
    图5 氯离子在砂浆中的扩散系数Fig.5 DRCM of chloride in mortar
    参考文献
    引证文献
引用本文

卢佳涛,孔丽娟,樊子瑞,谢书衡.铁尾矿砂-地聚物复合材料的界面与性能[J].建筑材料学报,2022,25(6):585-590